Description
Specifications
-
Growth Method: CZ
-
Dimensions: 5 × 5 × 0.5 mm
-
Orientation: (111)
-
Polishing: One side epi-polished (1SP), surface roughness Ra ~10 Å
-
Electrical Properties: N-type, Antimony (Sb)-doped, with a resistivity of 0.005–0.01 Ω·cm (If you would like to measure the resistivity accurately, please order our Portable 4 Probe Resistivity Testing Instrument.)
-
Package: Under Class 1000 clean room
Typical Properties
-
Structure: Cubic, a = 5.6754 Å
-
Density: 5.323 g/cm³ at room temperature
-
Melting Point: 937.4 °C
-
Thermal Conductivity: 60.2 W/m·K (at room temperature)