Description
- Single crystal SrTiO3, Nb:0.1 wt%
- Size: 10mm x 10mm x 0.5mm
- Orientation: (100) +/-0.5 o
- Polish: two sides polished.
- Surface finish( RMS or Ra): <5A
|
|
Typical Physical Properties |
|
Crystal Structure |
Cubic, a=3.905 A |
| Nb doping | 0.1 wt% |
|
Growth Method |
Vernuil |
|
Density |
5.175 g/cm3 |
|
Melt Point |
2080 oC |
|
Hardness |
6 ( Mohn) |
|
Thermal expansion |
10.4 (x10-6/ oC) |
|
Resistivity |
0.007 ~ 0.1 ohm.cm for 0.1 wt% Nb doped SrTiO3 |
|
Loss Tangent at 10 GHz |
~5x10-4 @ 300K , ~3 x10-4 @77K |
|
Color and Appearance |
Black |
|
Chemical Stability |
Insoluble in water |