Description
|
Typical Physical Properties |
Crystal Structure |
Cubic, a=3.905Å |
Growth Method |
Vernuil |
Density |
5.175 g/cm3 |
Melt Point |
2080 oC |
Hardness |
6 ( Mohn) |
Thermal expansion |
10.4 (x10-6/ oC) |
Dielectric Constant |
~ 300 |
Loss Tangent at 10 GHz |
~5x10-4 @ 300K , ~3 x10-4 @77K |
Color and Appearance |
Transparent (sometimes slightly brown based on annealing condition). No twins. |
Chemical Stability |
Insoluble in water |
|
STO is grown by the flame fused method ( Vernue ). So crystal perfection is not as good as the crystal grown by CZ, each substrate's Rocking curve may be different. Please always check STO substrate before growing the film. To understand why to please click " How to grow SrTiO3 crystal " |
|
|
![]() |