Description
- Fluorine-Tin-Oxide (FTO) coated Glass Plates ( Corning brand-TEC70 )
- Dimension: 100 x100 x 3.2 mm
- Nominal FTO Film thickness: <150 nm
- Resistivity: 58~72 ohm/sq
- Phi (work function): 4.83~5.03 eV (Kelvin probe)
- Visible Transmittance:82-84.5 %
- Haze: 0. 5%
- Heat Flow thru Glass: TEC 70 at 27 deg C/ air space/TEC 15 glass at -20 C: 86 W/m^2
- Heat Flow thru Glass: TEC 70 at 27 deg C/ air space/clear glass/air space/clear glass at -20 C: 94 W/m^2
|
|